OLS-3263 | Liquid Encapsulant - Two part Dimethyl Silicone

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

Compression Mold Phenyl Silicone Encap Optically Clear Two-Part Phenyl Silicone LED Liquid Encapsulant Phenyl Silicone Dispense LED Liquid Silicone Phenyl Encap PPA Package Phenyl Silicone Refractive Index 1.54

Main features

  • Dimethyl Silicone potting compound
  • Excellent UV and heat resistance
  • For the encapsulation of mid- and high-power LEDs

Product Description

Optically Clear Two-Part Dimethyl Silicone LED Liquid Encapsulant

OPTOLINQ OLS-3263 is a two-part (Part A & Part B), optically clear dimethyl silicone designed for the encapsulation of mid- and high-power LEDs. It features a very good heat resistance, high optical transmittance and excellent resistance to both UV and heat resistance in applications as high as 170°C. Dimethyl-type silicones are known to have an even higher optical transmittance and wide processing windows. It also has a high level of adhesion to a wide-range of metals, silicones and plastics and to PPA in particular. OLS-3263 can be dispensed from standard dispensing equipment or can also be compression molded using compression mold equipment.

Main Features

  • Two-part, optically clear dimethyl silicone for LED encapsulation
  • High optical transmittance with a wide processing window (dimethyl silicone platform)
  • Excellent UV + heat resistance for demanding light and thermal exposure environments
  • High-temperature capability in applications up to 170°C
  • Strong adhesion to many metals, plastics, and silicones; excellent adhesion to PPA
  • Scalable processing: compatible with standard dispensing and compression molding
  • Phosphor compatible (supports mixing for die-level color conversion)

Applications

OLS-3263 is specially designed for mid- and high-power LED devices, particularly where operating temperatures are higher and long-life reliability is critical, including:

  • Automotive lighting (high-temperature, vibration, long service life)
  • Industrial bay lights (warehouses, high ambient temperatures)
  • Street lighting / outdoor luminaires (thermal + environmental exposure)
  • High-power projectors / beamers (high intensity, long throw requirements)
  • Mid/high-power LED modules requiring clear encapsulation and robust adhesion
  • Phosphor-mixed encapsulation for die-level color conversion

 

Product Family

233172

500g Net Wt (250g Part A & 250g Part B) packaged in 500ml jars
1. Select Weight

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Unit of measure Bottle
Net weight 500 kg
Gross weight 550 kg
Dimensions 25 x 40 x 30 cm

Technical Specifications

Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
125 ˚C

Additional Information

OPTOLINQ Family series

KRAYDEN OPTOLINQ™ OLS-Series are a family of optically clear (often called “water-white”) liquid encapsulants that are used to encapsulate optical or optoelectronic devices that require both a high level of light transmittance as well as a good level of mechanical protection. Products in this OLS-Series family can be epoxies, silicones or hybrid technologies. They are used extensively for the encapsulation of LED devices, but could be well suited for other applications that require a clear, optical grade encapsulation system.

The OPTOLINQ OLS Series is KRAYDEN’s Opto Liquid System (OLS) series and is made up of several families of products that each have their own unique attributes and application-specific benefits.

OPTOLINQ Family Series

The OPTOLINQ OLS Series is KRAYDEN’s Opto Liquid System (OLS) series and is made up of several families of products that each have their own unique attributes and application-specific benefits.

Main Applications

  • Mid-power LED Encapsulation
  • High-power LED Encapsulation
  • Compression Molding LED devices
  • Compression molding opto lenses

Product Features & Benefits:

  • Temperatures up to 170°C
  • Excellent adhesion to PPA
  • Excellent Heat Stability
  • Excellent UV stability

Additional Handling Instructions

Preheat Part A to 40°C and then mix in Part B in the required mixing ratio given above. Ideally, the mixture of Part A and B will be done in a vacuum and degassed at 3 torr (400 Pa) for 10-15 minutes. This will ensure that all the entrapped air bubbles are removed after mixing. For best results, ensure that all moisture has been removed from the parts to be encapsulated by preheating them for 1 hour @ 90°C. Also for best results, the encapsulation should be carried out in a vacuum.

Using Additives with OLS-3263

Optolinq OLS-3263 can be mixed with diffusing agents or color pastes to achieve customer-specific purposes.

Recommended quantity (in weight %) of various diffusing agents and color pastes to be used with OLS-3263:

  • OAA1-2 Red Color Paste: 2-5% by weight
  • OAA1-3 Blue Color Paste: 1-3% by weight
  • OAA1-4 Green Color Paste: 2-4% by weight
  • OAA1-D Diffusing Agent: 2-5% by weight

Storage and Handling

OPTOLINQ OLS-3263 is supplied in cans and jars and should be kept in a cool (10°C – 25°C) dry place (40% – 75% humidity) away from direct sunlight or temperature extremes. Part B is particularly sensitive to moisture, so be sure to remove moisture after using and to keep the lid of the container tightly sealed after use.

For safe handling information on this product, consult the Safety Data Sheet, (SDS).

Data Ranges

The data contained herein may be reported as a typical value and/or range values based on actual test data and are verified on a periodic basis.

Leading Brands Trust in Our Products and Services