LOCTITE ECCOBOND UF 1175

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND UF 1175

Main features

  • White
  • Low CTE
  • Easy dispensability

Product Description

LOCTITE ECCOBOND UF 1175 partial, white epoxy underfill is formulated for use on large chip sizes, providing good UPH and reliability. Typically used as an electronics encapsulant and a circuit board underfill

LOCTITE ECCOBOND UF 1175 is a fast cure, monocomponent underfill with controlled flow. It offers low CTE and can be dispensed easily and without stringing.

Cure Schedule

  • 15 minutes @ 120°C
Product Family

233802

30cc Syringe - 2765900
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 64 days
CA Shipping in 12 weeks
EU Shipping in 60 days
Packaging
Unit of measure Syringe
Net weight 40 g
Gross weight 58 g
Dimensions 4.5 x 3 x 3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.65
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
154 °C
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
1.05
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
35,295 mPa.s

Leading Brands Trust in Our Products and Services